[MW:4380] ferrite number of duplex stainless steel weld

Hi,
We have a different understanding for the generally, the oil & gas industry, the percent ferrite should be between 35 - 60% and the FN from 4 - 8

We would assume you are using Ferritscope MP 30 for the measurement


David Chan
~~~~~~~~~~~~~~~~~~~~~~~~~~
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sukamal Naskar
Sent: Friday, February 26, 2010 1:22 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:4376] ferrite number of duplex stainless steel weld

Optimum is 50FN, but 40 ~ 70 FN will be acceptable , but still it
depends on the client's technical specifications.

Regards,

On 2/26/10, pankaj.johri@in.transport.bombardier.com
<pankaj.johri@in.transport.bombardier.com> wrote:
> Hi,
>
> We are welding duplex stainless steel.
>
> To control the parameters of welding, we are measuring ferrite number of
> weld.
>
> Can anybody tell us how acceptable values of ferrite numbers are decided.
>
>
> Regards,
>
> Pankaj
>
>
> Please consider the environment before you print / Merci de penser à
> l'environnement avant d'imprimer
>
> _______________________________________________________________________________________________________________
>
> This e-mail communication (and any attachment/s) may contain confidential
> or privileged information and is intended only for the individual(s) or
> entity named above and to others who have been specifically authorized to
> receive it. If you are not the intended recipient, please do not read,
> copy, use or disclose the contents of this communication to others. Please
> notify the sender that you have received this e-mail in error by reply
> e-mail, and delete the e-mail subsequently. Please note that in order to
> protect the security of our information systems an AntiSPAM solution is in
> use and will browse through incoming emails.
> Thank you.
> _________________________________________________________________________________________________________________
>
>
> Ce message (ainsi que le(s) fichier(s)), transmis par courriel, peut
> contenir des renseignements confidentiels ou protégés et est destiné à
> l?usage exclusif du destinataire ci-dessus. Toute autre personne est, par
> les présentes, avisée qu?il est strictement interdit de le diffuser, le
> distribuer ou le reproduire. Si vous l?avez reçu par inadvertance,
> veuillez nous en aviser et détruire ce message. Veuillez prendre note
> qu'une solution antipollupostage (AntiSPAM) est utilisée afin d'assurer la
> sécurité de nos systèmes d'information et qu'elle furètera les courriels
> entrants.
> Merci.
> _________________________________________________________________________________________________________________
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Sukamal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...