Thursday, February 4, 2010

Re: [MW:4210] RE: Painting internal of GVC

Dear friend:

What kind of vent condenser do you have?, which is the material of the tubes?, how it will enter sand into the system?... I think you just need to avoid the sand entering into the system, you have to remember that a condenser need is to have a high thermal potential, with a high conduction qualities material, so before protect by painting, you just need to protect the system backwards. Anyway, please give more details to bring you a better answer.
 
Best regards
 
Vladimir Lizama
Civil & Mechanical Engineer
2010/2/4 Qamlr <qamlr@cicb-chemicon.com>

Friends

 

Would you please give any recommendations for painting the internals of the Gland vent condenser where there is a possibility of SAND entering the system. Client location is in Middle least having corrosive atmosphere.

 

Thanks

 

Regards

 

Prashanth Hegde

 



Please don't print this e-mail unless you really need to.
*******************************************************************
This e-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return e-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.
*******************************************************************
"SAVE PAPER - THINK BEFORE YOU PRINT!"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...