Monday, February 8, 2010

[MW:4245] effect of Jacking for correction of ovality

dear all,
 
please inform me whether ANY CODE allows ovality correction in pipe/shell  by jacking.( Applying load  by Screw Jack).
 
What will be the effect of jacking.
 
what NDT Shall be perofrmed after jacking on the affected locations.
 
 
Thanks & Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...