Monday, February 8, 2010

[MW:4243] interpass temperature for SAW welding(by twin wire) of line pipe by API5L

Dear all
 
please inform me how we can check interpass in helical welding  for line pipe by Automatic SAW( twin wire).  what will be interpass temperature.
 
 base material is API 5L Gr. 65, thickness is  10.01 mm.
 
filler wire is L70 & Flux is P223.
 
welding requires impact testing. please inform me whether interpass is required to be checked or not.
 
Thanks & Regards
 
Asad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...