Saturday, February 6, 2010

[MW:4235] Availability of ER 80S B6L with max.carbon% 0.05

Our project requires ER 80S B6L filler wire with  Carbon percentage 0.05% max as per PMC's specification.
I have approached so many suppliers here in India but everybody quotes for 0.07% max.
Please suggest a supplier.
 
Hrishi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...