Wednesday, December 30, 2009

[MW:3917] WPS & PQR clarification

Dear Group
 
 Good day,
--------------------------------------------------------------------------------------------------------------------------------
Still I have confusion on WPS and PQR terms.
 
1. WPS to be created  first , with respect to  selection of process, electrode and current  etc.
2. PQR is developed  after WPS ,by entering the the actual variation  relevant to the WPS.
 
|Corresponding reference numbers are to be entered  in each other.
 
This is the information  from ASME IX codes.
 --------------------------------------------------------------------------------------------------------------------------
But there is a controvercial  statement  from some of our colleques, PQR to be developed first and  Supporiting PQR  reference number is to be entered in the WPS.
 
Please clarify this confusion .
 
 
mahendra
KSA
 
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...