[MW:3424] Re: prequalified wps

Again, you have to prove the equivalence.

--- On Sat, 3/10/09, Endri Prasetyo <endri.prasetyo@gmail.com> wrote:

From: Endri Prasetyo <endri.prasetyo@gmail.com>
Subject: [MW:3412] Re: prequalified wps
To: materials-welding@googlegroups.com
Date: Saturday, 3 October, 2009, 8:49 PM

Dear Ali,

Even this material is equivalent with some material, it shall be qualified.

Regards,
Endri

Powered by BlackBerry®


From: Ali Asghari <asghariali@rocketmail.com>
Date: Sat, 3 Oct 2009 05:31:27 -0700 (PDT)
To: <materials-welding@googlegroups.com>
Subject: [MW:3408] prequalified wps

Hi FRIENDS
is it possible to write a prequalified wps for ST37 according AWSD1-1?(THIS MATERIAL NOT LISTED IN TABLE 3-1,BUT HAVE SIMILLAR COMPOSITION WITH SOME LISTED )
REGARDS.







Yahoo! India has a new look. Take a sneak peek
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...