[MW:3416] SS316 mechanically lined API 5L Gr60 pipes

Dear All,

Please highlight me on the differences/ advantages / disadvantages of  SS316 mechanically lined API 5L Gr60 pipes in comparison with SS 316 clad ( metallurgically bonded ) API 5L Gr60 pipes.

Regards,

Mithun



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...