Monday, November 17, 2008

[MW:1318] Re: PWHT soaking time

Dear Friends,
 
Is a PQR with soaking time of 1 hrs can support a WPS  with soaking time 3 hrs. (No Impact requirement). 
 Ans: NO
Is a PQR with soaking time of 10 hrs can support a WPS  with soaking time 3 hrs. (No Impact requirement).
 Ans: YES

Regards


 
On 11/16/08, kataiah@bilfal.com <kataiah@bilfal.com> wrote:

Dear Friends,

Is a PQR with soaking time of 1 hrs can support a WPS  with soaking time 3 hrs. (No Impact requirement).
Is a PQR with soaking time of 10 hrs can support a WPS  with soaking time 3 hrs. (No Impact requirement).
Is a p

Regards

P.K
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...