Wednesday, November 12, 2008

[MW:1300] RE: 1299] Casting quality levels

MSS-SP-55

 

 

 

 

Best regards,
For Det Norske Veritas (USA), Inc.
William G. Davis
__________________________________
Head of Section - QA Services
Region North America
DNV ENERGY
Ph: 281-721-6621
Fx: 281-721-6909
Mob: 281-352-5462
e-mail: william.davis@dnv.com
www.dnv.com


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of rahul.pisat@akersolutions.com
Sent: Wednesday, November 12, 2008 9:05 AM
To: materials-welding@googlegroups.com
Subject: [MW:1299] Casting quality levels

 

Hello ,

 

Please guide about the definition of the Casting quality level .

Where I can find about the quality of casting as 1, 2 or 3.

 

Also I am not able to understand the Acceptance level ( or class ) specified in ASME 31.3 Table 302.3.3 D.

 

Where can I find this casting level defined ?

 

kind regards

Rahul Pisat

 


This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS