Tuesday, November 11, 2008

[MW:1293] Re: FITTINGS

You can propose 100% radiography on welds with UT as well to convince the client and get the deviation accepted by the client.The chances are however quite remote.Invariably the fittings are seamless upto 16"NB and welded,18"NB and above.
Regards
Aarpee

 
On 11/11/08, Raghuram Bathula <raghurambathula@gmail.com> wrote:

it is upto the designer/owner to accpet/reject and also depnds on the
time delays required to source new fittings. if these are used in
lines which are categorised as normal fluid service, you may approch
your client with a devaition request and probably with additional NDT
on the longitudinal welds of these fititngs.

On Nov 10, 10:22 pm, carlos oliveros <carlosolive...@terra.com> wrote:
>           BODY { font-family:Arial, Helvetica, sans-serif;font-size:12px; }
> Dears Friends.
>
>         I work in a project  Plant Compressor Gas under B31.3  The
> specification Project give the reference Fittings seamless and in
> Shop Fabrication the fitting are welded Elbow welded, Tee Welded. My
> question reject all fabrication or what is the solution.
>
>         Thanks
>  carlos oliveros --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...