Tuesday, November 11, 2008

[MW:1290] Re: Sec IX requirement for plug welds

hi
because types of weld stated in IX are groove & partially groove & fillet & spot,therefore i soppose you qualify your plug weld with groove weld(if your components retain pressure)otherwise by fillet .


From: CKPurohit <ck@knm-group.com>
To: materials-welding@googlegroups.com
Sent: Monday, November 3, 2008 11:20:37 AM
Subject: [MW:1266] Sec IX requirement for plug welds

Dear All,

 

Can somebody guide me what are the requirement for PQR qualification for plug weld.

 

I need to weld the plugs of SS liner on the Cr Mo Body (outer shell).

 

Regards.

CK


***DISCLAIMER NOTICE ***
"This e-mail and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above.
If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited.
If you receive this e-mail in error, please notify the sender immediately by return e-mail and delete the e-mail and any of its attachments.
Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...