Values can be different however values to be achieved in Weld Metal are with respect to desired values of parent metal.If Impact values achieved for Weld Metal are within the acceptable range as specified for Parent metal then there is no issue.What is further more important and critical is the values achieved in Heat Affected Zone.HAZ is the area which undergoes critical changes in microstructural phases with respect to cooling rate of weld metal.
Regards
Aarpee

 
On 11/10/08, Sudipto_Banerjee@fwuk.fwc.com <Sudipto_Banerjee@fwuk.fwc.com> wrote:

Can anyone tell me whether the impact test value will be same for the
parent metal and the weld metal? or it can be different.

Best Regards,
Sudipto Banerjee
Man. no. B 4974
Equipment Engg. Department
Office no. 0044- (0)118 913 2295


=======================================================
Confidentiality Notice

This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com.
=======================================================





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...