Please refer QW 382.2.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of CKPurohit
Sent: 06 November, 2008 6:00 AM
To: materials-welding@googlegroups.com
Subject: [MW:1272] RE: 1270] Re: Sec IX requirement for plug welds

 

Dear Carlos,

 

Construction code is Sec VIII (so we need to follow Sec IX) Vessels are code stamped.

 

P No for Cr Mo is P4 and for SS is P8 Gr 2

 

But the info I need only for plug welds which clause to be referred in Sec IX to find out PQR and performance qualification requirement.

 

Regards.

CK

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of carlos oliveros
Sent: Sel, 04 Nov 08 08:11 pm
To: materials-welding@googlegroups.com
Subject: [MW:1270] Re: Sec IX requirement for plug welds

 

Hi, CK, What is the construction standard. ASME IX , Section II is the guide.

What Number P SS is P8 and Cr Mo pending the percent Cr Mo(P4, P5).

Give information more

carlos oliveros

On Mon 03/11/08 03:50 , "CKPurohit" ck@knm-group.com sent:

Dear All,

 

Can somebody guide me what are the requirement for PQR qualification for plug weld.

 

I need to weld the plugs of SS liner on the Cr Mo Body (outer shell).

 

Regards.

CK


***DISCLAIMER NOTICE ***
"This e-mail and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above.
If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited.
If you receive this e-mail in error, please notify the sender immediately by return e-mail and delete the e-mail and any of its attachments.
Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."


</HTML


***DISCLAIMER NOTICE ***
"This e-mail and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above.
If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited.
If you receive this e-mail in error, please notify the sender immediately by return e-mail and delete the e-mail and any of its attachments.
Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...