Skip to main content

[MW:700] pabitra das wants to chat

-----------------------------------------------------------------------

pabitra das wants to stay in better touch using some of Google's coolest new
products.

If you already have Gmail or Google Talk, visit:
http://mail.google.com/mail/b-7a01d2baae-e5a17d912b-9eb5389ce5526cc7
You'll need to click this link to be able to chat with pabitra das.

To get Gmail - a free email account from Google with over 2,800 megabytes of
storage - and chat with pabitra das, visit:
http://mail.google.com/mail/a-7a01d2baae-e5a17d912b-7cb0b1086d

Gmail offers:
- Instant messaging right inside Gmail
- Powerful spam protection
- Built-in search for finding your messages and a helpful way of organizing
emails into "conversations"
- No pop-up ads or untargeted banners - just text ads and related information
that are relevant to the content of your messages

All this, and its yours for free. But wait, there's more! By opening a Gmail
account, you also get access to Google Talk, Google's instant messaging
service:

http://www.google.com/talk/

Google Talk offers:
- Web-based chat that you can use anywhere, without a download
- A contact list that's synchronized with your Gmail account
- Free, high quality PC-to-PC voice calls when you download the Google Talk
client

Gmail and Google Talk are still in beta. We're working hard to add new features
and make improvements, so we might also ask for your comments and suggestions
periodically. We appreciate your help in making our products even better!

Thanks,
The Google Team

To learn more about Gmail and Google Talk, visit:
http://mail.google.com/mail/help/about.html
http://www.google.com/talk/about.html

(If clicking the URLs in this message does not work, copy and paste them into
the address bar of your browser).

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

The Schaeffler and Delong diagrams for predicting ferrite levels in austenitic stainless steel welds

Introduction Ferrite is important in avoiding hot cracking in during cooling from welding of austenitic stainless steels. 'Constitution diagrams' are used to predict ferrite levels from the composition by comparing the effects of austenite and ferrite stabilising elements. The Schaeffler and Delong diagrams are the original methods of predicting the phase balances in austenitic stainless steel welds. Nickel and chromium equivalents A 'nickel equivalent' is calculated for the austenite stabilising elements and a 'chromium equivalent' ferrite stabilising elements. These are used as the axes for the diagrams, which show the compositional equivalent areas where the phases austenite, ferrite, martensite (and mixtures of these) should be present. Although intended to show the phase balance of weld fillers, these diagrams can also be used to illustrate the phase balance of the 'parent' material. There are different diagrams for dif...