Skip to main content

[MW:651] Fugitive emission test equipment

Test equipment for what ? (i mean to test the facility, equipment or component) or you want a simple gas analyser comonly used by HSE personnel? or hifi equipment like Infrared Gas Imaging and Quantification Camera

Is it a construction site or a running process plant, where you are looking for complete LDAR solutions?

for e.g. API MPMS 19.3 PART D covers Test Method for the Measurement of Deck-Seam Loss Factors for Internal Floating-Roof Tanks

fugitive emissions from equipment in facilities that use, manufacture or transport toxic and dangerous fluid products are genearally requested for valves (ofcourse valves are the single largest source for this emissions), sealing systems used in rotating machinary (for e.g could be pump shaft sealing or compressor or could be a mechanical seal of reactor etc.)

it is very important for any piping class/material specialist to look in to this requirement while selecting the materails like gaskets or any sealing material, surface finish of flange etc.


-----Original Message-----
From: Ramesh C [mailto:cramesh1971@gmail.com]
Sent: Mon 03/03/2008 20:27
To: materials-welding@googlegroups.com
Subject: Re: [MW:632]

can any body send the details of *Fugitive emission test equipment*

**
Thanks & regards,
Ramesh.C
L&T, KPM-site


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .