[MW:683] Re: Section IX QW 200.4(b)


Yes Sanjeev
 
U can use GTAW for root deposit as per QW 200.4b.
 
shabbir
 
On 3/21/08, jitendra Thakor <jitendrathakor@gmail.com> wrote:

Dear Sanjeev

As per QW200.4(b) it is mandatory that your GTAW PQR thickness should
be minimum 13 mm. than you use GTAW as root as qualified in PQR.

Regards
Jitendra

On Fri, Mar 21, 2008 at 2:11 PM, sajeev c.g <sajeevmech@yahoo.com> wrote:
> Dear all,
>
> I have to prepare a WPS from two PQR's as per section IX.
> PQR 1 qualified in 10mm coupon full GTAW
> PQR 2 qualified in 40mm coupon SMAW+SAW(20mm deposit each)
>
> Can i write a WPS to weld GTAW (root) + SMAW+SAW?
> As per QW200.4(b) is it mandatory that the PQR 1 will be qualified in 13mm
> minimum to write a WPS as above?
>
> Regards
> sajeev
>
>  ________________________________
>
> Looking for last minute shopping deals? Find them fast with Yahoo! Search.
> >
>
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .