Skip to main content

[MW:669] Re: [MW:/] tolerance for CE

Dear Mustak,
 
There is no requirement of C.E in ASME. In fact code is not asking for C.E, its we as per our requirement and services going for C.E
 
Shabbir

 
On 19 Mar 2008 04:05:09 -0000, mustak patel <mustak_patel123@rediffmail.com> wrote:

 
Hi guys

What is the tolerance given in the AMERICAN CODES for CE value for applicability of WPS and welder qualifications? Is it an essential variable? I think in British or japanese standards its given + 0.003 % Max.

Appreceiate any feed back.

Thanks and Regards


On Tue, 18 Mar 2008 rajesh patel wrote :
>
>dear Friebds,
>
>I am a silent but regular reader of the mails shared
>by group memebers. I am greatful to receive such
>valuable information from the various people from
>every corners of the world. Through this group,I even
>recd some mails from my old couligues with whom i lost
>all contacts since last so many years.
>
>I may not be replying or sharing anything but i am
>very much interested to receive such mails. Whenever
>it feels necessary, I will definately contribute.
>
>Pl continue to send me mails.
>
>Regards,
>
>Rajesh B. Patel
>QC Engineer
>Adyard Abudhabi LLC
>
>--- "Bathula Raghuram (Mumbai - PIPING)"
><R.Bathula@ticb.com> wrote:
>
> > No exchange of information since last 1 week, that's
> > why you were not
> > receiving any mails.
> >
> > Appreciate your concern and request members for
> > their active
> > participation.
> >
> >
> >
> > -----Original Message-----
> > From: donboscomarine@vsnl.net
> > [mailto:donboscomarine@vsnl.net]
> >
> > Sent: Tuesday, March 18, 2008 12:10 PM
> > To: materials-welding@googlegroups.com
> > Subject: Re: [MW:659] Bolt Length in ASME B31.3
> >
> >
> >
> > Dear Mr. Bathula Raghuram,
> >
> >
> >
> > We are not getting any communication since 12th
> > March, 2008. Before
> > that, we were witness to a very good exchange of
> > information. Any reason
> > for non-receipt of communication or is it just that
> > there has been No
> > Exchange? Will like to know the cause. We are
> > impressed by the quality
> > of information exchange and consider ourselves lucky
> > to have been a
> > memebr of this group.
> >
> >
> >
> > We will be obliged if a reply is sent ASAP.
> >
> >
> >
> > Thanks & B. Rgds.
> >
> >
> >
> > G. A. Soman
> >
> > Principal
> >
> >
> >
> >
> >
> >
> >
> >
> >
> > DON BOSCO MARITIME ACADEMY
> >
> > Premier Automobiles Road,
> >
> > Kurla West, Mumbai 400070
> >
> > Tel:  (022) 2504 1585 / 2018.  Fax: (022) 2504 0682
> >
> > Email:  donboscomarine@vsnl.net
> >
> > Website: www.dbma.in
> >
> >
> >
> >
> >
>
>
>
>      ____________________________________________________________________________________
>Be a better friend, newshound, and
>know-it-all with Yahoo! Mobile.  Try it now.  http://mobile.yahoo.com/;_ylt=Ahu06i62sR8HDtDypao8Wcj9tAcJ
>
>
>>



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .
Honda