[MW:10763] RE: 10750] chemical value for C,P,S

ASME Sc IIC, 2010 ed., SFA-5.1 Table 7 

e.g.

C  <  0.15

Mn < 1.60

Si  < 0.75

P/S < 0.035

Ni < 0.30

Cr < 0.20

Mo < 0.30

V < 0. 80

[Mn + Ni + Cr + Mo + V] < 1.75

 

John

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of senins welo
Sent: Wednesday, April 20, 2011 7:54 AM
To: materials-welding@googlegroups.com
Subject: [MW:10750] chemical value for C,P,S

 

Dears sirs,

            For AWS A 5.1 E7018,The chemical composition  for C, P, S VALUES not specified in ASME SEC 2 ,PART C, WHAT IS THE VALUE? WHERE?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...