What your client spec says? if client spec ask for RT and you want to go with UT, this would call for "Specification Deviation Request".
Regards
Manpreet Singh
On Mon, 07 Feb 2011 09:21:27 +0530 Ali Asghari
>
Dear All
>we have a distribution line that contain gasoline. now is there code case or other standards that allowed radiography replaced by ultrasonic. ( the size of pipe is 8'')
>in ASME b31.8 the criteria of radiography is API1104, but it's not mentioned extent or replacing.
>Regards
>
>we have a distribution line that contain gasoline. now is there code case or other standards that allowed radiography replaced by ultrasonic. ( the size of pipe is 8'')
>in ASME b31.8 the criteria of radiography is API1104, but it's not mentioned extent or replacing.
>Regards
>
>
>
> --
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment