Re: [MW:9749] Carbon Steel weldability

If it goes for pwht after welding ,better use ER 70S-A1(1/2Mo) or ER80S-G (1/2Mo)
Pandithan

On Sat, Feb 5, 2011 at 10:39 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,

I have 2 questions :

 1-  For one Boiler construction project, we have to weld carbon steel
material (SA 106 Gr b), the client WPS precise that we will use ER80SG
Gtaw filler metal.

 I just request when & why  this filler metal is required for Carbon
steel, why we don't use ER70S3 or ER70S6.


 Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...