Dear Srinivas,
 
Welder can be qualified in 3G Position using ur 4G WPS, no issue in that.
 
No need of Qualifying WPS in 3G further .
 
Regards
Anil
On Tue, Feb 1, 2011 at 4:27 PM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear all.

I have a qualified WPS in 4G.
Can i qualify welders to 3G position as per 4G wps without WPS
qualification?
Pl advise me. Its urgent.

Thanks
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...