Hi.

First which code you have to follow as per client requirement,
2. ASME. AWS, BS or BIS or API as like you have to see. there will be
some variations here and there will be there.
3. check the base material MTC for physical / chemical impact results.
4. Accordingly check with ASME Sec II Part C check the welding
consumables composition.
5. Compare the base metal and welding consumables variables.

if all make pwps as per your codes.

carry out welding as per PWPS and test mechanical properties.

If the results are ok prepare PQR and from this PQR you can prepare WPS
and production could be followed .

best of luck.



On Tue, 01 Feb 2011 13:34:46 +0530 wrote
>Dear experts, Could you please give some guidelines or codes,
references on how to prepare WPS & PQR? I'm sure your valuable inputs
will help me to prepare this.Thank you,Ilan
**********************************************************************B
orouge is a leading provider of value creating, innovative plastics
solutions for customers in the Middle East, Asia-Pacific and Africa.
Borouge employs unique Borstar® technology to produce differentiated
products for high-value infrastructure applications, including water,
gas and industrial pipe systems, power and communication cables,
advanced packaging and automotive components. Borouge's state-of-the-
art petrochemical complex is located at Ruwais, Abu Dhabi in the United
Arab Emirates.
=======================================================================
============
>CONFIDENTIALITY NOTICEThis email and any files transmitted with it are
confidential and intended solely for the use of the individual or
entity to whom they are addressed. If you have received this email in
error please delete the email and any attachment(s) and notify the
sender.This footnote also confirms that this email message has been
scanned for the presence of computer viruses.
>======================================================================
======================================= 




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...