RE: [MW:9629] Weld Repair on PTFE lined vessel

It is SS-316, 2” NB vessel design Code is B-31.3

 

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Tuesday, February 01, 2011 1:06 PM
To: 'materials-welding@googlegroups.com'
Subject: RE: [MW:9624] Weld Repair on PTFE lined vessel

 

What is the code and material of construction?

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vinod Kataria
Sent: Tuesday, February 01, 2011 12:42 PM
To: materials-welding@googlegroups.com
Subject: [MW:9622] Weld Repair on PTFE lined vessel

 

Dear All,

Please see the attached photo for the undercut and advice if it is possible to repair this on PTEF lined vessel the vessel. The size is 2” NB and wall thickness is 2mm with inside PTFE lining of 4mm. We have imported this vessel from Germany but during 3rd party inspection it is rejected because of this undercut. The working pressure of this vessel is only 3.5 bar and its successful withstood a hydro test pressure of 10 bar.

Now I request all the expert to please advice if we can repair this undercut if yes than please provide me some guideline or some procedure to carry out this repairing.

Thanks in advance for your kind help.

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...