Just to add as per AWS D1.1 the weld types requiring qualification.


Inline image

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Saturday, 10 June, 2023 at 05:38:01 pm IST, mithlesh kumar <mithleshmech47@gmail.com> wrote:


Dear James,

Attached table is for position qualification , Only in case of T,Y & K Type joint fillet can performed. Please correct me if I am wrong.


Thanks
Mithlesh

On Thursday, June 8, 2023 at 5:35:11 PM UTC+5:30 james gerald wrote:
Details like plate,  position etc.. required. Decode from the below snapshot of AWS D1.1

Inline image
Inline image



Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Thursday, 8 June, 2023 at 12:13:04 pm IST, Parminder Singh <parms...@gmail.com> wrote:


WPS qualified in CJP as per AWS D1.1 Ed 2020 

On Thu, Jun 8, 2023 at 11:57 AM Baqer Shabbeer <engb...@gmail.com> wrote:
Please share here qualification's and design code

On Wed, 7 Jun 2023 at 1:58 PM, Parminder Singh <parms...@gmail.com> wrote:
Dear Experts, 

Will CJP WPS qualify for Fillet Welds ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8bee16cf-540c-431a-a8b2-b5409547abd1n%40googlegroups.com.
--
Regards,
Baqer Shabbeer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJBr9BGRACOA%2BKgyT7v9xDveXiOT9UOqJPgEamV0B91Doso78Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/bd5eed17-01c5-4f91-9a2c-d6fae0d74d9fn%40googlegroups.com
.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .