Skip to main content

Re: [MW:34297] Impact test requirement for Unlisted material (ASTM A707 L5 CL3)

Thanks for your all response, 
we done the impact at -55°C in PQR, My query is our service fluid is water and service temp is 0° to 90°C, i believe then the thickness range in WPS we can use 5 mm to 50.4 mm.  
Design Code: B31.3
Qualification Standard : ASME Sec IX

On Monday, June 12, 2023 at 6:06:35 AM UTC+3 james gerald wrote:
ASTM A707 L5 forged product material impact tested at -60degC But API 5L X65  material for a thickness of 50.8 require Impact tests as per ASME B31.3 and hence PQR shall be impact tested

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Saturday, 10 June, 2023 at 05:37:53 pm IST, aravind roche <aravin...@gmail.com> wrote:


Experts,

please advise below,  I believe because of our service temperature the impact test is not required, please guide me. 

PQR material - A707 L5 CL3 to API 5L Gr X65
Thickness coupon: 25.4 mm
WPS qualified range is : 5 to 50.8 mm
Design code : B31.3
Qualification Standard : ASME Sec IX
Our Project MDT : 0° to 90°C
Service : Water
PWHT : Yes
Pre heat : Yes

Aravind.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ec3be245-165e-41a9-a0a2-40f333501774n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7560590a-02d8-4cdc-931e-db926a941addn%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...