It's regarding Simulation PWHT.

Question- how to prepare 3 cycle Simulation PWHT for SA387 Gr. 11. Low Alloy Steel? 
How to select soaking time and temperature for three cycle. 

Regards, 
Navanath Kashid. 

On Thu, 8 Jun, 2023, 10:23 AM , <materials-welding@googlegroups.com> wrote:
Sunthar Ambikapathy <sunthar1974@gmail.com>: Jun 07 11:32AM +0530

Dear Quality Team,
 
 
 
Pl provide suitable electrodes for as attached PMI composition.
 
 
 
I was selected for the E11018 electrode. With Preheat 150 deg.
 
 
 
What is your option.., and welding procedure ?
 
 
 
Equipment : Air receiver Header ,Size Dia 250mm X 4mm.
 
Application : ESP / Bag filter pulsing header.
 
Services : 12 years old, power plant .
 
Defect: Fillet weld center of portion crack observed.
 
Chinese Power Plant.
 
 
 
 
[image: image.png][image: image.png]
 
 
 
 
--
Kind Regards
 
Sunthar A
+91 9894100888
Shahil Saini <sainishahil98@gmail.com>: Jun 06 07:38PM +0400

Hello everyone,
Good Evening,
hope all are doing well,
 
As my subject indicates PWHT in SS to CS Weld joint, my question is what
are the after effects if pwht performed in SS to CS joint??
 
In Addition, how to mitigate the after effects which occurred after pwht?
 
BM: SS 316L to SA516 Gr.70
Parminder Singh <parmsin2001@gmail.com>: Jun 07 03:32AM -0700

Dear Experts,
 
Will CJP WPS qualify for Fillet Welds ?
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B8p7iWo69OQhr3e6dJawswMr71%3D2NT2_jAtyBVsrLhnsqX7mg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...