Re: [MW:34262] Weld Rejection Rate (WRR) for Welder and Welding Operator

Hi
According to ISO and EN standards, there are no requirements for WRR.
ISO 9001 says you have to control only the parameters you describe or which are involved in good production and have a direct impact on quality.
Only according to project specifications and internal company experience.
2023 m. birželio 5 d., pirmadienis 11:12:40 UTC+3 Hải Trần rašė:
First is project specification relate
Second is project procedure relate
This issue didn't mention on any standards

Vào Th 2, 5 thg 6, 2023 lúc 12:23 s.navaneethan.mani <s.navanee...@gmail.com> đã viết:

Hi expert ,

 Anybody aware of the international reference standard of weld rejection rate for welders /welding operators .

image.png


Thanks & Regards

Navaneetha Perumal S

QA/QC Engineer -Mechanical & Welding

CSWIP 3.1, NDT Level-II & ISO 9001

M :+966-505721787 (WhatsApp & Calling)            M :+919750521128

ThinkGreen before printing this email.

10 Liters of water is required to produce one sheet of A4 paper


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOj8udN5y-%2BSutP1Tg8CqY50yQS6_-DjohkP2JZ_w%3DiAmOiF0Q%40mail.gmail.com.
--

 

Best & Regards


Hai, Tran Ngoc (Mr.) / QA/QC Engineer
Mobile +84-977-881-880/ +84-948-614-951

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/726fb019-e348-4fa1-aa9f-9ae79e3f93c7n%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...