What type of Gasket is and what are the torque values applied? (it should be backed by calculations suitable with the gasket, bolts/flange material, lubrication etc.)
Buckling may cause turbulence in fluid flow, and may leak over time.
On Fri, 29 Jul 2022 at 13:23, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Pl ur inputs on the below mail.--THANKS & BEST REGARDS,KG.PANDITHAN, BE, IWE, CSWIP 3.1,ISO 9712 Level 2 in VT,ASNT-Level II in PT,MT,RT & UT,LA ISO 9001-2015,International Welding Engineer.CONSULTANT-WELDING & QUALITYMobile no: +919940739349---------- Forwarded message ---------
From: Ponnikumar <k.ponni1994@gmail.com>
Date: Thu, Jul 28, 2022 at 5:55 PM
Subject: Flange tightening
To: Kannayeram Gnanapandithan <kgpandithan@gmail.com>Dear sir,I have a doubt in flange tightening in our project work 6" flange cl900# NRV flange type valve we did hydraulic torquing the gasket bent (bucking) to touch flange inner surface . So client inspector reject due to this I ask what criteria based on reject nothing reply get from himPlease help me to solve this issue any code have or not?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMs2bDbPm7X3fcv3FO_EfJcfDF48x-AhCxuxtu8mhDOzg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DBQswqkWiX%2B1L8G_p_7mzRh-usCZmy71-vonaBgik4zg%40mail.gmail.com.
Comments