Re: [MW:33301] Pickling and passivation need before painting SS surfaces

Glass-Bead blasting is recommended for SS.

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 26 July, 2022 at 01:05:58 pm GMT+4, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


I suppose you do sweep blasting before Painting and there is no purpose for Pickling and Passivation.

Thanks & Regards

J.Gerald Jayakumar



On Tuesday, 26 July, 2022 at 12:19:01 pm GMT+4, Anilkumar G <akg.nitt@gmail.com> wrote:


Dear Experts

Do we need pickling and passivation of SS surfaces before painting them? Could you please suggest any specification relevant this requirement?
The parts are SS cast valves requiring painting.

Regards
Anilkumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/754e0d61-54e1-420e-ae4b-f92593266f5en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1830374327.1245268.1658826084959%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...