Re: [MW:33282] Back gouging

Yes , its non essential parameter you can revise the WPS

On Fri, 22 Jul 2022 at 10:44, sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear experts,

We have Qualified WPS Sa516 grade 70 with GTAW +SMAW  with out back gouging.........my Question is can we weld a plate with Back gouging..??



Best Regards
Sujit kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWNf2qnd--LWzua4jkGTd2qggp_sOui5JnMX6UWbT6RGSw%40mail.gmail.com.
--
Pravinkumar kurade

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM02rkcpBh-A4KoH_zD9Pt7CJW-fBu3u%3DGVBNWDsMFwW85T2yw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...