Re: [MW:33282] Back gouging

Guys,

Check in ASME if back gouging is essential variable(perhaps not) for welding process used and then decide.
Usually adding back gouging it is accepted.

Regards

Gigi

On Friday, 22 July 2022 at 08:48:49 EEST, srinivas rao <engr.srini@gmail.com> wrote:


Yes, you can do if it is only ASME , but check your client specification if your client specification calls for seperate welding procedure, prepare a WPS for the process by which you are going to do and incorporate both the single Side and  double side groove designs in  WPS submit for client approval.


Regards 
Srinivas Rao
Welding Engineer 

On Fri, Jul 22, 2022, 9:39 AM madheswaran s <madhes.sss@gmail.com> wrote:
Yes u can ...

Sent from my iPhone

On 22-Jul-2022, at 10:44 AM, sujit kumar <sujitkumar19942@gmail.com> wrote:


Dear experts,

We have Qualified WPS Sa516 grade 70 with GTAW +SMAW  with out back gouging.........my Question is can we weld a plate with Back gouging..??



Best Regards
Sujit kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWNf2qnd--LWzua4jkGTd2qggp_sOui5JnMX6UWbT6RGSw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0A104ACF-B754-4015-A3A2-DFBC3935DAEC%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHdRSOMNLPEveBi6qhHm4Q5qCGd8KNEgfB-o%3D5eNN0K5pBviZQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...