Though Pulsing is mentioned as a non-essential variable for GTAW, WPS is a document for Welder to follow apart from Approving. Hence necessary details shall be mentioned.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 20 July, 2022 at 02:38:05 pm GMT+4, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


SMAW & SAW no Pulsing.

Only GTAW & GMAW pulsing.


It depends on your Machine capability in adjusting the below.

Peak current & Time
Background Current & Time

Upslope & Downslope

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 20 July, 2022 at 12:22:37 pm GMT+4, madheswaran s <madhes.sss@gmail.com> wrote:


Dear Experts, 

What to write the in the wps , where pulsing current ------- mentioned

iF i use SMAW process in wps pulsing current -------
iF i use GTAW process in wps pulsing current -------
iF i use SAW process in wps pulsing current -------
iF i use GMAW process in wps pulsing current -------

What to write for each procss , 

Can one one tell the answers as mentioned avove.(Applicable/not applicable/none/yes etc.)

Thanks.
Madheswaran.S

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/36fd9ece-5234-42e9-b1e1-fd3900b1d214n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/228151060.2128663.1658311276651%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...