The electrode baking shall be as per the consumable manufacturer recommendations. This can't be generalised, we all know.
If customer specification allows baking more than once, at the same time if the electrode manufacturer is also ok for baking a second time, you can do it. Go for it. 

On Sat, Jul 16, 2022 at 6:34 PM madheswaran s <madhes.sss@gmail.com> wrote:
Dear Experts, 

I have a question about baking of electrodes. spec or other says backing of electrodes only one time. Now my question is if i received electrodes carton box from manufacturer Like E7018 ok, If  baking the electodes then we maintain the elecrodes in holing oven the issuesd to welder for welding, If some electodes are not used , they are exposed in atmosperic condition about 8 hrs, In this case can i do baking again? or already once we backed the elecrode before issuing to welder, so we can't back again? because once only baking permitted. I dont know clear understand ? can anyone help this case.
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4b3918f2-ec32-4a7f-9d04-6ce30107b9dbn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKMJiNXjQqVFcrC5UxpCQS6KUED-CtWqfQDfjJP%2BVhHNv8QgEw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...