Saturday, July 16, 2022

Re: [MW:33257] Baking Electrods only one time, but how ?

Baking of lowhydrogen electrodes can be done 1 time only making sure that it will all be used in production welding, however if happen to have some leftover those can remain in the holding oven and make sure to use first in line, if not should be discarded rightaway. 



On Sat, 16 Jul 2022 at 9:04 PM madheswaran s <madhes.sss@gmail.com> wrote:
Dear Experts, 

I have a question about baking of electrodes. spec or other says backing of electrodes only one time. Now my question is if i received electrodes carton box from manufacturer Like E7018 ok, If  baking the electodes then we maintain the elecrodes in holing oven the issuesd to welder for welding, If some electodes are not used , they are exposed in atmosperic condition about 8 hrs, In this case can i do baking again? or already once we backed the elecrode before issuing to welder, so we can't back again? because once only baking permitted. I dont know clear understand ? can anyone help this case.
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4b3918f2-ec32-4a7f-9d04-6ce30107b9dbn%40googlegroups.com.
--
Anthony Dipasupil Dalisay
TWI AWeldI

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALBzUBK074q8xocaXz%3DBZyv29kpDUzcH9UsoXTo462GL%2BdZHTg%40mail.gmail.com.

No comments:

[MW:35692]