u have to match minimum tensile strength. in ur case, 516 gr 70 means minimum tensile is 70000psi or 485 Mpa. To match this, u can very well use 7018 which is 70000 psi or 485 Mpa. U are not supposed to match with actual tested value because it will vary. 

On Fri, Jul 15, 2022, 11:53 AM Kishore S <kishore.sk002@gmail.com> wrote:
Dear sir 

what are the step to find an electrode for SA516 gr 70 in the internet they have mentioned E7018 but as per the SAIL TEST CERTIFICATE tensile strength is 79ksi so what electrode do I have to use   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ab5513fa-c564-40ce-953a-f67e68a3ea03n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNnOT-e7FcVShxuWpr5zonhuK_XE8Ugr6y_fdK%3DhX9LTw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...