Re: [MW:33248] Additional Joint

Yes you can. Consult with your design team for this.
Weld according to a qualified WPS.
You may need RT for the full length joint after forming and after heat treatment if applicable.

Regards
Anilkumar

On Fri, Jul 15, 2022 at 11:29 AM CKML <chaitanyakamal@gmail.com> wrote:
Dear Experts 

 Can i proceed forming of 30 mm thk Plate by joining of 2 Plates for  Lower shell dish end.

If cant what would be the acceptable of joining length of plates.
If yes what precaution to be take care.

Any reviews 

can any one help me 

Regards
chaitanya kamal 
ph-8226081506  



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/57bd9e9a-da16-4e1c-ba2b-dc806d01205bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKMJiNUjn2mXaYz1bR4fzOcdwk-vTe2MMp79z%2BOxcbZYjcdfng%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...