Re: [MW:33241] WELDER QUALIFICATION REQUIERMENT

So he is qualified  for  weld deposit in production Welding for 

GTAW = 10mm maximum
SMAW=18.54 mm maximum

The essential variables of WPS, WPQ shall be  checked and followed during production Welding.



On Thu, 14 Jul 2022, 14:47 Adnan Ziad, <adnanziad49@gmail.com> wrote:
GTAW 5 mm
SMAW 9.27mm

On Thu, Jul 14, 2022, 09:02 Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Welder qualification range is independent of thickness  range of WPS s.

What is his weld metal deposition qualification
GTAW ___mm??
SMAW __mm??



On Thu, 14 Jul 2022, 13:18 QA/QC, <adnanziad49@gmail.com> wrote:
Dear Experts

i have two wps's for piping cs/ltsc welding with the asme b31.3 ans sec 9  one thickness range is 3 to 20 mm and the second is 20.01to 31.22  pwht requiered .the two is GTAW+SMAW

i have a welder qualify in test coupon 6'' 14.27 mm 

my question is this welder will qualify to weld in the two wps or we should make another qualification for him seperately 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/083762d2-dd64-482a-85e9-0e4f7aa4e14bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P0oXvwk645wv4SsUdJfwqRyPNSg7raKpXV-4sAVaK_VA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACbfGKdM8HLVPsXdcWwXMnFrNLMvp2L7c4q-zcjUmGZvUpbieg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NKri%3DaB5X8c0SF0eFy8BptNYwT2HaVEOC9BZU3Ptp0nA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...