Saturday, July 30, 2022

[MW:33324] Need support for gas cutting and welding ,shot blasting and painting costing.

Dear All Experts
Please help me ,I want to do actual costing (for arc and CO2 welding)of gas consumption,electrode consumption,CO2 wire consumption.If have any data please share. .
Regards
Sachin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOsVSySZ_ckO8Bw6Z%3DgS0Yaozo7mJF-cQqiHmfJ4rvu_3K8NZg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...