Thursday, April 8, 2021

Re: [MW:32192] Procedure for the welding Electrode testing

1.Welding process - butt weld (  metal arc welding )
2.AWS Classification: E6010, E7010
3.Diameter of electrode : E6010 - 2.5-3.2MM
                                              E7010- 2.5-3.2MM
On Wed, 7 Apr, 2021, 18:50 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Normally procedure will be available for storage Conditioning and Handling of welding electrodes.

Welding electrode testing is available in ASME Sec.IIC.

If you want to be specific please provide the below details

1. Welding process
2. AWS Classification for eg like E 7018 etc..
3. Diameter of welding electrode

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 7 April, 2021, 05:14:28 pm IST, tejas kerzare <tejas.kerzare3@gmail.com> wrote:


Dear All,

Can you please provide me the procedure for welding electrode testing to weld  seamless carbon steel pipe API 5L Grade B.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPv03FuKVxo269jwyd%2B_%2BGy0h4KPqanPXiZQn-HbsCAb5LqKkA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20094860.181083.1617799879540%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPv03Fv-jN_dXtQ_%2BwhBcDR-gtFH77_VJTOMmfNxod-t838DTQ%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...