On Thu, Apr 8, 2021 at 5:31 AM Xuân Thông <xuanthong.hp@gmail.com> wrote:
Hi sir,I think it is better if you show the drawing. Our friends can support you easily--Vào Th 5, 8 thg 4, 2021 vào lúc 10:09 EmaD FaRaHanI <emad.farahani@gmail.com> đã viết:--Dear all,
Considering we want to weld the inspection box in a water-cooled chimney for a fume hood in a steel plant. The tubes are a nominal diameter of 2 inches, SA210 mild steel (tubing material) with a wall thickness of approximately 0.22".
1-What welding processes were used to butt weld the tubes to create the inspection opening in the fume hood?
2-would you give me a welding symbol?
3-What NDT method is better for inspection of fillet welds on the inspection box metal casing?
Thanks,
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJFxtqqVK1mSxdvqRU3G%2BWjMnSLft7igf5nX7s7kqF7aZw%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OnicZfHDCGfyKikC3%2Bzr5SytMzB47nPoUW6MV_mNPeVVA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJF1HaTMp6FdEY3ow%3DpH_Y_5Jxp5BfgBwCsdoWbJUHk4%2Bw%40mail.gmail.com.
No comments:
Post a Comment