Thursday, April 8, 2021

Re: [MW:32188] Welding process and NDT method for fillet welding

Hi sir,
I think it is better if you show the drawing. Our friends can support you easily


Vào Th 5, 8 thg 4, 2021 vào lúc 10:09 EmaD FaRaHanI <emad.farahani@gmail.com> đã viết:

Dear all,

Considering we want to weld the inspection box in a water-cooled chimney for a fume hood in a steel plant. The tubes are a nominal diameter of 2 inches, SA210 mild steel (tubing material) with a wall thickness of approximately 0.22".

1-What welding processes were used to butt weld the tubes to create the inspection opening in the fume hood?

2-would you give me a welding symbol?

3-What NDT method is better for inspection of fillet welds on the inspection box metal casing?

 

Thanks,

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJFxtqqVK1mSxdvqRU3G%2BWjMnSLft7igf5nX7s7kqF7aZw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OnicZfHDCGfyKikC3%2Bzr5SytMzB47nPoUW6MV_mNPeVVA%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...