Thursday, April 8, 2021

[MW:32184] Welder qualification record for all Weld cladding and weld overlay materials

Dear All,

Please share a Welder qualification record, test reports & JCC Card  for all Weld cladding and weld overlay materials

And how to Qualified Multi qualification for one welder like Range ,Thickness, Dia and  All materials.

Any special NDT requirements for welder Qualification like mechanical test and  ndt as per Sec 9 & API 1104.

Difference as per Sec 9 & API 1104. ( Piping And Pipeline ) 

Like materials.
1.Carbon Steel to weld clad or weld overlay Materials.
2.Carbon Steel to 625 and 825 Nickel based Alloys.
3.Carbon Steel to Copper based Alloys.
4.Carbon Steel to Stainless materials.
5. And also Any other Special weld clad or weld overlay materials..

Thanks in Advance,
PKM..

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nc2QAroxtrECf8cYSoPGmHBQaGxJ%3DDAda%2B%3Duz5QD0A1aQ%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...