Wednesday, April 7, 2021

Re: [MW:32184] Welding Carbon steel

Hi sir,
Please find the attached WPS for your reference

Vào Th 4, 7 thg 4, 2021 vào lúc 15:17 Mohammed Jazril k k <jazril.shinu@gmail.com> đã viết:
Dear friends,

From the following welding methods, Any one suggest me which welding can be used for welding CS pipe fittings such as elbows and 90 degree bends of SCH 40, and Size of 60".............for water line. 

          1) FCAW
          2) GTAW
          3) SMAW 
          4) GTAW + SMAW

Thanks & Regards
Mohammed Jazril

On Tue, 6 Apr, 2021, 10:52 AM Mohammed Jazril k k, <jazril.shinu@gmail.com> wrote:
Dear sir

Thank you for your mail and reply,

The material used for the job is carbon steel of sch 40....

Thanks & Regards
Mohammed Jazril


On Tue, 6 Apr, 2021, 8:49 AM Xuân Thông, <xuanthong.hp@gmail.com> wrote:
Dear Sir,
your above mentions mean WPS for GTAW + SMAW of pipe line ? Please let me know what material to be used ?

Vào Th 2, 5 thg 4, 2021 vào lúc 19:20 Mohammed Jazril k k <jazril.shinu@gmail.com> đã viết:
Dear sir

Anybody can share the estimation data sheet for GTAW & SMAW welding process in a pipe line.......

Thanks & Regards
Mohammed Jazril

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKTgLOSMBjNPLS-v5GJWpz7E_G5GCfCoawkqL6gZfDCyWNLOHQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OmPdH0uB9yh43b6r2Dr2f7j_JpZ-QXC9h1pqOy4LH8foA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKTgLOSj-j5Lt8nMJC3mbZjUAiK_FRHELqStkhqjSx0g51D_Ww%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OnJdUfu%2B4Ns%3D3d-FsrBhRZYRJjor8yjeG1paXYAnuNFOA%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...