Wednesday, April 7, 2021

Re: [MW:32183] Welding rod

Based on the availability. If you weld carbon steel with SS316L, E309MoL is a better option.

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 7 April, 2021, 07:42:08 pm IST, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


Why 309LMo

On Wed, Apr 7, 2021, 7:28 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Try using E309L or E309MoL

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 7 April, 2021, 06:55:25 pm IST, alading <alla.benachi@gmail.com> wrote:


Dear all
Is it possible to weld carbon steel using stainless 316L rod 

Thank you 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B%3DJkv1iSea1jyar9Gg%3D%3DGMZoRL5gW7dZO44aP0KWJvm6QDL0A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1303319381.192783.1617803039685%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN9KgBW9KD68ipDbs_zfkBA5cnnHrZ2FTK%3DR98gkMPGww%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...