Dear Sir,
I think that is specified by the project specification or inspection and test procedure
On the other hand, you can refer to others standard AISC or ISO 13920 for the acceptance criteria of dimensional
Vào Th 2, 5 thg 4, 2021 vào lúc 09:36 Sandeep Pr <prsandeep61@gmail.com> đã viết:
--Dear Friends,Can anybody give me the Reference for Column Base Plate Distortion Tolerance.SHS(Built Up member) is welded to base Plate(CJP).With Regards,Sandeep
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFBEtQq3bs_pUd%3DaETz%2Bdf5uWWooi6YLVewf8iO-FGqRzU_KyQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OkOT0U3SrXi9TkYdAKTAQJYKu3yC8LApFoKpAiEVoNHMg%40mail.gmail.com.
No comments:
Post a Comment