Re: [MW:32157] interruption limitations to stop welding

Hi sir, 
The stop welding may be to check any cold cracking if any prior to weld the next layers

Vào Th 5, 1 thg 4, 2021 vào lúc 13:51 sankar krishnan <sankar.bombay@gmail.com> đã viết:
Dear All ,

  In our Pressure vessel project 10mm thickness plate they using (GTAW+SAW) process , They have welded GTAW with 4 mm of 10mm thickness and leave open for 1 days .. I like to Know what is the interruption limitations to stop welding Limits for <19mm thickness 

Please send me code documents 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ca6ac61-bff9-444e-bc40-80249c545c8dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OnvpqSTuyQp%3DpdpvtNQB_mouo-4B7R5bnUr0Aty6dMshQ%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...