On Mon, Apr 5, 2021 at 5:36 AM QA/QC <adnanziad49@gmail.com> wrote:
Hey mastersi want to know about the selection of tank plate material with thickness in storage tank of oil with 5000 m3 capacitythere is any formula or its just from api 650 -620--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5a309c35-f239-4da7-b118-180950941e19n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHbaPvKOLHNicwwdGZ56BQpehXeBFibxG87KdrqJuHFR%2Bm7Ciw%40mail.gmail.com.
No comments:
Post a Comment