Monday, April 5, 2021

Re: [MW:32153] storage tank plate selection material and thickness

good morning,

API 650 have the formula

Kishor 

On Mon, Apr 5, 2021 at 5:36 AM QA/QC <adnanziad49@gmail.com> wrote:
Hey masters 
i want to know about the selection of tank plate material with thickness in storage tank of oil with 5000 m3 capacity 

there is any formula or its just from api 650 -620 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5a309c35-f239-4da7-b118-180950941e19n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPd%2B2RQm%3D6LgZ-nxB9Sg0TGBbj3ou%2B-YvvMK2wQzoR0muQVX-g%40mail.gmail.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...