Brother 
   What about stress concentration and Oxidation of weld material , fast cooling at open atmosphere, How they will maintain the interpass temperature to avoid delay cracks 
these are the thing to be considered for low thickness , if i am wrong let me correct myself 

On Thu, Apr 1, 2021 at 3:10 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
referring code
If it is ASME, no restriction
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Apr 1, 2021 at 12:21 PM sankar krishnan <sankar.bombay@gmail.com> wrote:
Dear All ,

  In our Pressure vessel project 10mm thickness plate they using (GTAW+SAW) process , They have welded GTAW with 4 mm of 10mm thickness and leave open for 1 days .. I like to Know what is the interruption limitations to stop welding Limits for <19mm thickness 

Please send me code documents 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ca6ac61-bff9-444e-bc40-80249c545c8dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePc_h0Rk2n-fKNTrrC4YvyqgU-mJ7ru-URZQJe_qL%3Dh3w%40mail.gmail.com.


--
shankar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyDEebuMQiz2h%2B%3DqnEbqH3-wOt0J8LyOfw4Caj6dk1iGrzgsg%40mail.gmail.com.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone